Modified ring compression tests on 42-lb. linerboard. Project 1108-32, a preliminary report to Technical Committee of the Fourdrinier Kraft Board Institute, Inc.
Modified ring compression tests on 42-lb. linerboard. Project 1108-32, a preliminary report to Technical Committee of the Fourdrinier Kraft Board Institute, Inc.
dc.contributor.corporatename | Institute of Paper Chemistry (Appleton, Wis.) | en_US |
dc.contributor.corporatename | Fourdrinier Kraft Board Institute, Inc. | en_US |
dc.date.accessioned | 2004-09-08T16:29:27Z | |
dc.date.available | 2004-09-08T16:29:27Z | |
dc.date.issued | 1963-09-03 | en_US |
dc.description | "September 3, 1963." | en_US |
dc.format.extent | 351250 bytes | |
dc.format.mimetype | application/pdf | |
dc.identifier.uri | http://hdl.handle.net/1853/1394 | |
dc.language.iso | en_US | en_US |
dc.publisher | Appleton, Wisconsin : the Institute, | en_US |
dc.publisher | Georgia Institute of Technology | en_US |
dc.relation.ispartofseries | Institute of Paper Chemistry (Appleton, Wis.). Project 1108-32 ; preliminary report [September 3, 1963] | |
dc.subject.other | Kraft liner boards. | en_US |
dc.subject.other | Compression tests | en_US |
dc.subject.other | Ring crush resistance | en_US |
dc.subject.other | Ring crush tests | en_US |
dc.title | Modified ring compression tests on 42-lb. linerboard. Project 1108-32, a preliminary report to Technical Committee of the Fourdrinier Kraft Board Institute, Inc. | en_US |
dc.type | Text | |
dc.type.genre | Project Report | |
dspace.entity.type | Publication | |
local.contributor.corporatename | Institute of Paper Science and Technology | |
relation.isOrgUnitOfPublication | 6c27e726-78e5-4645-8d27-6b6724df05af |
Files
Original bundle
1 - 1 of 1